QUANTITY OF PARTS TO BE INJECTED BY ALUMINIUM QUALITY

Material

Temp. of Material (ºC)

Temp. of Mold (ºC)

Injection Pressure (in bar)

Pressure maintained (in bar)

AW 5083 Cast

Certal® / SPC

Alumold®

Hokotol®

Polietileno BD (PEBD) 160 - 260 20 - 70 500 - 1000   ●● ●●●● ●●●● ●●●●
Polietileno HD (PEHD) 260 - 310 50 - 70 600 - Max 30 - 100% ●● ●●●● ●●●● ●●●●
Polipropileno (PP) 250 - 270 40 - 100 600 - Max 50 - 100% ●● ●●●● ●●●● ●●●●
Poliestireno (PS) 180 - 230 20 - 60 1000 - Max   ●● ●●●● ●●●● ●●●●
Poliestireno CHOC (PSC) < 250 45 - 60     ●● ●●●● ●●●●  
SAN 220 - 260 50 - 70 1000 - Max   ●●●● ●●●●  
ASB 220 - 280 60 - 80 800 - 1400   ●●●● ●●●● ●●●●
Poliamida 6/6 (PA 6/6) 250 - 290 80 - 90 700 - 1200 30 - 100% ●●●● ●●●● ●●●
Poliamida 6 (PA 6) 240 - 290 80 - 90 800 - 1300 20 - 60% ●●● ●●● ●●●
Poliamida 11 (PA11) 230 - 300 30 - 90 400 - 700   ●●● ●●● ●●●
POM 180 - 220 50 - 120 800 - 2000 PI ●●● ●●● ●●●
PC 270 - 320 80 - 120 800 - 2000 70% ●●● ●●● ●●●●
PETP 260 - 270 140 1200 - 1700   ●●● ●●● ●●●●
PETP amorphous 270 - 290 70 - 80 1000 - 2000   ●● ●●●● ●●●● ●●●●
PBTP 260 - 270 40 - 50 1200 - 1700 60 - 100% ●● ●●●● ●●●●  
PPO 260 - 300 80 - 110 1000 - 2000 60 - 80% ●● ●●●● ●●●● ●●●
PVC 170 - 190 50 - 60 1200 - 1400 50 - 80% ●● ●●●● ●●●●  
PMMA 200 - 250 40 - 90 500 - 2000   ●● ●●●● ●●●● ●●●
PA 6/6 + fiberglass 260 - 290 90 - 120 900 - 1500 40 - 100% ●● ●● ●● ●●●
PA 6 + fiberglass 240 - 290 90 - 120 1000 - 1500 20 - 60% ●● ●● ●●●
PC + fiberglass 300 - 325 90 - 110 1000 - 2000 70% ●● ●● ●●●
●●●● 1.000.000 a 2.000.000 (Large qtt series) ●●● 100.000 a 500.000 (Medium qtt series)
●● 10.000 a 50.000 (Small qtt series) ● up to 5.000 parts